Recommended Printing Settings
| Drying Settings (Blast Drying Oven) | 70 °C,8 h |
| Printing and Keeping Container's Humidity | < 20% RH (Sealed, with Desiccant) |
| Nozzle Temperature | 220 - 240 °C |
| Bed Temperature (with Glue) | 30 - 35 °C |
| Printing Speed | < 80 mm/s |
Physical Properties
| Density | 1.16 g/cm³ |
| Vicat Softening Temperature | N / A |
| Heat Deflection Temperature | N / A |
| Melting Temperature | 185 °C |
| Melt Index | 5.2 ± 0.3 g/10 min |
Mechanical Properties
| Tensile Strength | 29.6 ± 0.6 MPa |
| Breaking Elongation Rate | > 700% |
| Bending Modulus | N / A |
| Bending Strength | N / A |
| Impact Strength | N / A |
Accessory Compatibility
| Recommended | Not Recommended |
| Build Plate | Cool Plate, Engineering Plate, High Temperature Plate or Textured PEI Plate | / |
| Hotend | Hardened Steel Nozzle 0.4 / 0.6 / 0.8 mm) Stainless Steel Nozzle (0.4 mm) | Stainless Steel Nozzle (0.2 mm) |
| Glue | Bambu Liquid Glue Glue Stick | / |
Printing Tips
• TPU needs proper drying before printing, recommended drying temperature is 70 ℃ for 8 hours in a blast drying oven, or 90 ℃ for 12 hours on a printer's heatbed. For more details please refer to Filament drying cover on WIKI.